WIND CYCLING
Wind Dynamic Load (100-hour Continuous) by location
Wind-speed variation data over 100 hours converted to a current-density schedule (0 to 0.78 A/cm2) and applied to our bifunctional NiCo electrode in an AEM cell with a commercial Zirfon separator. ΔV before/after LSV at 0.5 A/cm2: 20 mV.